Flying Whale H06-4 Epoxy Zinc-rich Antirust Paint

Product overview

With epoxy resin and polyamide resin as the base material, zinc powder as the anti-rust pigment two-component epoxy zinc-rich anti-rust paint, paint film has excellent durability and rust resistance, paint film toughness has good impact resistance, wear resistance, oil resistance and water resistance, and has a cathodic protection effect.

Recommended use

Industrial protective paint field:
It is used for the surface of industrial structural parts with high anti-corrosion performance requirements, and is suitable for high-performance anti-rust primer for large bridges, port machinery, heavy equipment, petroleum refining plants, power plants, various steel structure equipment and facilities, etc.

Product Information

Color
Grey
Gloss
No light
Component B (curing agent) H06-4 epoxy zinc-rich paint curing agent
Volumetric solids 60±3%
Recommended dry film thickness 60 microns/approx. 100 microns wet film thickness
Theoretical coating rate 4.76 m2/kg (60 micron dry film meter)
Volatile Organic Compounds (VOC) 375g/L
DensityNote
Approximately 2.1kg/l
Note: Density data are typical parameters and vary with color

Dry data

Substock temperature 5 ℃ 10 ℃ 23℃ 35℃

Paint film surface dry

Solid paint film

Fully Cured

Mixed life

3 hours

24 hours

20 days

8 hours

2 hours

16 hours

14 days

6 hours

1 hour

10 hours

7 days

4 hours

0.5 hours

6 hours

4 days

3 hours

Overcoating data

Substock temperature 5 ℃ 10 ℃ 23℃ 35℃

Minimum coating interval

24 hours

16 hours

10 hours

6 hours

Maximum coating interval Months (when zinc salt is not formed on the surface of the paint film)

Note: 1. The above data are for reference only. The actual drying time and the length of the re-coating interval depend on the film thickness, ventilation, humidity, lower paint and mechanical strength, etc.

2. The surface of the paint film before recoating must be clean and dry, free of pulverization and other pollutants. If necessary, the surface before recoating should be fully napped.

Construction parameters

Mixing Use a power mixer to stir component A evenly, and then add component B while stirring until fully mixed.
ripening At the temperature below 10 ℃, aging for 15 minutes
mixing ratio Component A: Component B = 9:1 (weight ratio)
Thinner/cleaning agent Flying Whale X-103 Thinner
airless spraying

Nozzle diameter: 0.48~0.59mm

Nozzle pressure: 15 ~ 25MPa

Dilution ratio: 0 ~ 5% (by weight)

Gas spraying The use of suitable special equipment, spraying when the need for dilution
Brush/Roller Applicable, recommended for pre-coating and small-scale coating

CONSTRUCTION CONDITIONS

The substrate temperature shall be at least 3 ℃ higher than the air dew point, and the relative humidity shall be lower than 85%. The measurement of temperature and humidity should be carried out at the substrate near the operation point. When the construction is not in an open space, good ventilation must be provided to ensure the normal drying of the paint film.

Surface treatment

NEW STEEL: Blast cleaned to class Sa2.5 or hand sanded to class St3.

Steel coated with shop primer: secondary derusting shall be carried out to Grade St3.

Painted surfaces shall be clean, dry and intact on a compatible primer.

Typical supporting

H06-4 epoxy zinc-rich antirust paint 1 x 60 microns (dry film thickness)
H06-1 epoxy mica intermediate paint 1 x 120 microns (dry film thickness)
S43-38 aliphatic acrylic polyurethane topcoat 2 x 40 microns (dry film thickness)

For more scope of use, please consult Flying Whale New Material Company.

Safety and Health

Before using this product, please pay attention to the safety label on the packaging container, refer to and follow the information and precautions related to health and safety in the product safety technical manual of flying whale new material company. During the construction and drying of the product, appropriate ventilation and preventive measures must be adopted to control the solvent concentration within the safety limit to prevent poisoning or hypoxia. Take measures to avoid skin and eye contact with the product. If contact occurs, wash it immediately with suitable detergent, soap and water. If splashed into eyes, rinse with water and seek medical treatment immediately.

Packing specification

  Packing barrel specification Packing weight
Group A 20 Litres 31.5kg
Component B 5 Litres 3.5kg

Storage period

Store in a cool, dry, ventilated and dedicated warehouse away from heat sources. Under normal temperature conditions, the storage period is 12 months, and then it needs to be used after passing the inspection.

Precautions

The surface of zinc-rich primer is easy to form zinc salt (that is, basic zinc carbonate, commonly known as "white powder") when exposed to outdoor for a long time, so it should not be exposed for a long time before coating the post-coating. If a longer coating interval is required, it is recommended to apply epoxy micaceous iron intermediate paint as a closed coating as soon as possible to reduce the workload of secondary rust removal.

Corporate Statement

The above information and data of this product are accumulated according to our test and actual use experience, which can be used as a construction guide. For the construction carried out without our knowledge, we only guarantee the quality of the paint itself and are not responsible for any product performance problems arising from other aspects. We have the right to modify this manual according to the continuous improvement of the product.

Supplementary Notes

Film thickness and coating rate

dry film thickness wet film thickness Theoretical coating rate
50 micron 83 micron 5.71 m2/kg
70 micron 117 micron 4.08 m2/kg

 

Key words:

The bottom of the ship and the waterline parts with anti-fouling requirements.

Waterline and freeboard

Deck part

Superstructure

Ballast tank

Living Cabin

Battery compartment

Drinking water tank

Pretreatment of steel plate

Oil tank

More products


Leave us a message


Submit
%{tishi_zhanwei}%